14 Common Welding Defects, Causes and Remedies

A welder in welding

The welding process is a tricky one during the fabrication process. It has to be perfect otherwise the finished piece would be useless. However, like any other process, defects in welding are quite common. Welding defects are simply the defects of welding that can either be external or internal.

Well, there are many types of welding defects, and so are the causes of welding defects. But what are these? Don’t worry. We will tell you all the common welding defects and their causes and will try to give the remedies to cater to these defects as well.

Types of Welding Defects

Mainly, there are two types of welding defects based on their visibility. They are external welding defects and internal ones.

External DefectsInternal Defects
These defects are usually on the surface of the metal, and you can see them with your naked eyes.These defects are internally present in the metal after welding and you cannot see these defects with your eyes.
These faults are identified visually or through non-destructive welding inspection techniques, like magnetic particle inspection.You need to inspect thoroughly through different non-destructive and destructive welding inspection tests, like radiographic testing.
Examples: Undercutting, cracks, porosity, overlaps, and many othersExamples: Incomplete fusions and penetrations, slag inclusions

Welding Defects List: 14 Common Welding Defects

There are more welding defects than you think. We have explained 14 common welding defects, causes and remedies.

1. Porosity

Porosity

Porosity

When the air or bubbles of gas get stuck in the weld, it’s called porosity, also known as wormholes weld.

The gasses that get trapped are usually carbon dioxide, steam, and hydrogen. Looking at the porous weld, you feel as if it is a sponge with air bubbles in it.

These pours can be at a certain small area of weld or spread across the entire weld. The air bubble trapped inside makes the welded surface exposed to damage and corrosion.

Causes of porosity:

  • Very hot electrode
  • Electrode has more moisture than required

Remedies:

  • You need to keep the electrode dry and warm to minimize porosity.
  • Keep the current low.
  • Reweld or grind the weld with porosity.
  • Use appropriate electrodes like medium carbon steel and alloy having low hydrogen electrode.

2. Excessive Penetration

Excessive Penetration

Excessive Penetration

Excessive penetration means that the welded metal extends in a large quantity from the root of the weld. It causes bulging at that point and can severely cause corrosion and erosion.

Causes of excessive penetration:

  • Improper use of electrode
  • When the welding pool becomes overheated.
  • The type and size of the operating electrode are incorrect.
  • Large root gap.

Remedies:

  • Just like porosity, use minimum current.
  • Choose the right size and type of electrode.
  • The root gap should not be large.

3. Undercut

Undercutting

Undercutting

Undercut happens when a groove is formed in the weld metal base that spreads along the weld seam. T

here could be two causes of the undercut. The first one being too much current being used that leads to joint ends melting and draining into the weld. And, the second one is there is not enough filler metal in the weld. It decreases the cross-sectional area and produces grooves and notches. This, in return, adds stress under fatigue.

It is usually a beginner’s fault done by a naive welder or when multi-welds are performed at the fusion face. There are three types of undercuts: inter-run undercuts, continuous undercuts, and intermediate undercuts.

Cause of undercuts:

  • Using excessive current that causes overheating of parent metal.
  • Electrodes are kept for less time at the corners during weaving.
  • Shifted welding centerline.

Remedies:

  • The speed of the weld must be kept low.
  • Use low current during the whole welding process.
  • Fully clean plates before welding.
  • Give proper time for penetration at the edges.

4. Slag Inclusion

Slag Inclusion

Slag Inclusion

During welding, when some non-metallic particles get trapped in the weld, it forms a welding defect called slag inclusion. These non-metallic particles harden and form an external layer on the weld. This type of welding defect is usually in SMAW, flux-cored welding, and SAW.

Causes of slag inclusion:

  • When excessive weaving is done.
  • Used current and heat input is very low.
  • The weld pool is not as hot as needed.

Remedies:

  • Reweld or grind the weld to fix the issue.
  • Clean the plates and prepare them well so that the slag runs along smoothly without obstruction.
  • Increase the amount of current.

5. Lack of Penetration

Lack of penetration

Lack of Penetration

Incomplete penetration or lack of penetration is when the welded metal is not precisely fused into the base metal’s joint. There are different causes of lack of penetration.

Causes of lack of penetration:

  • The current is low.
  • Welding travel speed is high.
  • Preheat on low heat.
  • Edge preparation is incomplete.

Remedies:

  • Use higher current.
  • Carefully prepare the edges to achieve the appropriate thickness.
  • Keep the welding speed steady, not too fast.

6. Cracks

Cracks

Cracks

It is one of the most dangerous external welding defects that have the ability to grow bigger and spread across the entire length of the metal surface. It is also called lamellar tearing. They are very commonly present in tee and butt joint welds. You can see two types of weld cracks: transverse along the width and longitudinal forming parallel to the bead.

Moreover, there are two forms of cracks or lamellar tearing. When the welding temperature reaches 10K°C, hot cracks will occur and the weld will crystallize.

This can happen because of using the wrong filler material or because of sudden heating and cooling during the laser welding process. When the weld is completed and the material cools, cold cracks will occur. These cracks may take hours and even days to appear.

Cause of cracks:

  • High strength of joint.
  • You have chosen an incorrect welding technique.
  • Rate of cooling is high.
  • The electrode used is wrong.

Remedies:

  • Try weaving motion.
  • Employ different sequences during welding.
  • Choose an electrode based on the base metal.
  • Cooling of the welded part should be gradual.

7. Spatter

Spatter

Spatter

When tiny metallic droplets are spread all over the parent metal during welding, the defect is called spatter. These small particles came out from the welding arc.

This is one of the common welding defects frequently seen in arc welding, gas welding, MIG welding, and tack welding. You can also see this defect in welded joints.

Causes of spatter:

  • Very strong current.
  • Longer arc used.
  • Wet electrode.

Remedies:

  • Use low current amperage.
  • Produce slight arc.
  • Make sure that the electrode is dry.

8. Lack of Fusion

Lack of Fusion

Lack of Fusion

Overlapping or lack of fusion when the weld is not cohesive between the base and filler metal. It occurs when the filler, instead of joining and filling, starts flowing over the base metal.

Causes of lack of fusion:

  • The plates are not clean.
  • Improper fluxing.
  • The temperature is very low.

Remedies:

  • You must clean the plates before welding.
  • Choose the best welding technique and ensure all welding parameters are proper.

9. Concavity or Convexity

Concavity and convexity

Concavity and Convexity

These are welding defects where the weld makes a face from the toe and forms a dome-like structure. The curve of the weld faces inwards if it’s concave. Meanwhile, the face curve is outwards in case of convex fault.

Causes of concavity and convexity:

  • Welding speed is not maintained.
  • The current supply is inadequate.

Remedies:

  • Grind or blend the faulty weld to improve the fault.

10. Misalignment

Misalignment

Misalignment

When the two welded metal sheets or pipes are not exactly aligned, these types of welding defects are called misalignment. The misaligned weld can be seen with the naked eyes. It will have an uneven surface.

Causes of misalignment:

  • Welding fit-up is not right.
  • The thickness of the plates is not similar.

Remedies:

  • Choose plates with the same thickness to avoid misalignment.
  • For better appearance, grind and reweld the misaligned surface.

11. Mechanical Damages

If indentations appear on the base metal, it’s usually mechanical damage. It mainly happens when the technique, materials, and tools you use are not appropriate.

Causes of mechanical damage:

  • The electrode holder is mistreated.
  • The grinder is not used right.
  • Too much force applied.
  • Arc not attached to the metal.

Remedies:

  • Double-check that the electrode holder is controlled well.
  • Avoid aggressive hammering, and don’t do hammering if not needed.
  • Use welding tools with care.

12. Underfill

Underfill

Underfill

Underfill is the unfilled line that appears on the base metal when the welded metal doesn’t fill that part properly. This is one of the common external welding defects and can easily be identified by the naked eye.

Causes of underfill:

  • Welding speed is fast.
  • Heat input is quite high.
  • The welding technique is inappropriate.

Remedies:

  • You should use a weld gauge to inspect bid height from time to time.
  • Reweld the undercut portion.

13. Burn-Through

Burn-through

Burn-through

The types of welding defects that happen when due to high stress and heat, the weld bursts through the center and base metal melts, creating a hole as well.

Also called melt-through, this welding defect is visible and can be checked by the welder himself. Burn-through occurs in metallic sheets having a thickness of less than ¼ inches.

Causes of burn-through:

  • The welding torch is moved too slowly.
  • Metal pieces to be welded have a huge distance between them.
  • Heat input is high.

Remedies:

  • Avoid setting the current very high.
  • Keep the metal pieces side by side without too many gaps.

14. Excessive Reinforcement

Excessive reinforcement

Excessive Reinforcement

It is entirely the opposite of underfill welding. When the welded material fills too much, it causes overfilling or excessive reinforcement.

Causes of excessive reinforcement:

  • Wrong joint fit-up.
  • Too excessive current.
  • The welding is done at a very slow speed.

Remedies:

  • Grind the excessive filling.
  • Use appropriate joint fit-up.

Difference Between a Welding Discontinuity & Welding Defect

You might think welding discontinuity is the same as a welding defect. But these two terms are different. How? Let’s see through a comparison table:

Welding DiscontinuityWelding Defect
Any break in the normal flow of the weld is called discontinuity.A series of discontinuities that actually damage the finish is called a welding defect.
It occurs because of a wrong technique or pattern.There are multiple causes of welding defects.
This can be prevented and easily handled.You need to perform certain tests to detect them and fix them afterward accordingly.
Less severe than welding defects.More severe than discontinuities.

Detection of Welding Defects

There are different techniques you can try to detect all types of welding defects. The primary two categories are non-destructive welding inspection and destructive welding inspection.

Multiple tests come under each of these two inspection techniques. Let’s see what they are and how they can be used to detect a certain welding fault.

Non-Destructive Welding Inspection

When the inspection is done without physically damaging the weld. Mostly, it is done by the welder himself instead of a weld inspector.

Though the non-destructive tests are very precise and give accurate results, you need to make sure that a skilled inspector is performing them. And, if the welder is doing them, he/she should be very experienced.

Visual Inspection

The external welding defects that are easily detected visually. You don’t require any specific tools or equipment for visual inspection. Cracks, burn-through, undercutting, overfill etc can be easily detected visually.

While it is the easiest welding inspection method, it cannot detect internal defects. For that, you need to use the methods discussed below.

Dye Penetrant Testing

Also known as liquid penetrant testing, this method uses a fluorescent dye to detect microscopic lamellar tearing (cracks) that are too tiny for the naked eye to identify.

It’s an easy test to do and you need to pour a colored dye on the weld surface and let it dry for sometime. After drying, colored cracks will appear. Like visual inspection, it doesn’t detect advanced level internal defects.

Magnetic Particle Testing

A strong magnetic field is created around the weld, and the welding defect is identified using a magnetic probe placed at the ends of the weld.

Accumulation of small particles means there is a welding defect. The only drawback is that this method has limited application and can only be performed for some metals.

Ultrasonic Weld Inspection

During this inspection, ultrasonic high frequency rays are passed through the entire weld, which reflects back in case of defects. This test not only tests surface defects but also internal deformities as well.

Radiographic Weld Inspection

Just like ultrasonic testing, here, X-rays are passed through the welded surface, and a visual photograph is made on the attached screen like a human X-ray showing the place and type of welding defect.

Destructive Welding Inspection

The destructive testing techniques involve physically carving or damaging the weld in order to detect welding faults. Most of these tests are performed by the trainers to obtain certificates.

Some of the important destructive tests are:

  • Macro etch welding inspection
  • Transverse tension welding inspection
  • Guided band test

Conclusion

So, there you have it. We have explained 14 common welding defects, causes and remedies to so that you can cater to the welding defects and minimize them in your upcoming welding projects.

You need to be highly skilled and experienced to reduce the risks of defects. In case they happen, understand the ways to fix them. But even before fixing them, you need to check welding quality through any of the non-destructive and destructive testing.

Welding is a tricky process and needs to be done safely and perfectly. So, make sure you deliver high-quality welded pieces that can be used further in the fabrication process without any welding defects.


Frequently Asked Questions

1. What is the most frequent welding defect?

A: Porosity is recognized as a welding defect seen most often. This defect occurs when gas is enclosed in the weld, forming bubbles and subsequently reducing joint strength.

2. How do you find welding defects?

A: Welding defects can be found with the help of visual weld inspection, dye penetrant testing, ultrasonic testing, radiographic testing, and many other methods. You can choose according to the defect type.

3. What causes welds to crack?

A: Poor welds caused by incorrect welding, rapid cooling, and poor choice of electrode can cause the weld to develop cracks. If there is too much trapped stress in the weld joint, cracks can occur easily.

4. Are welding defects correctable?

A: Yes, many welding defects can be repaired by processes like grinding and rewelding, and adjusting appropriate welding parameters. Proper preparation and thorough welding inspection before welding can help prevent defects.

5. How is a welding defect different from a welding discontinuity?​

A: Discontinuity is the general term to describe an interruption in the weld structure. A defect occurs when the discontinuity becomes so severe that it starts to adversely impact the weld’s strength, quality, and performance.